Microwave Sol–Gel Synthesis of CaGd2(MoO4)4:Er3+/Yb3+ Phosphors and Their Upconversion Photoluminescence Properties
Автор | Лим, Ч. С. | |
Автор | Атучин, В. В. | |
Автор | Александровский, А. А. | |
Автор | Молокеев, М. С. | |
Автор | Орешонков, А. С. | |
Автор | Lim, C. S. | |
Автор | Atuchin, V. V. | |
Автор | Aleksandrovsky, A. S. | |
Автор | Molokeev, M. S. | |
Автор | Oreshonkov, A. S. | |
Дата внесения | 2016-11-11T08:54:04Z | |
Дата, когда ресурс стал доступен | 2016-11-11T08:54:04Z | |
Дата публикации | 2015-10 | |
Библиографическое описание | Лим, Ч. С. Microwave Sol–Gel Synthesis of CaGd2(MoO4)4:Er3+/Yb3+ Phosphors and Their Upconversion Photoluminescence Properties [Текст] / Ч. С. Лим, В. В. Атучин, А. А. Александровский, М. С. Молокеев, А. С. Орешонков, C. S. Lim, V. V. Atuchin, A. S. Aleksandrovsky, M. S. Molokeev, A. S. Oreshonkov // Journal of the American Ceramic Society. — 2015. — Т. 98 (№ 10). — С. 3223-3230 | |
ISSN | 00027820 | |
URI (для ссылок/цитирований) | https://elib.sfu-kras.ru/handle/2311/28053 | |
Аннотация | CaGd2(MoO4)4:Er3+/Yb3+ phosphors with the doping concentrations of Er3+ and Yb3+ (x = Er3+ + Yb3+, Er3+ = 0.05, 0.1, 0.2, and Yb3+ = 0.2, 0.45) have been successfully synthesized by the microwave sol–gel method, and the crystal structure refinement and upconversion photoluminescence properties have been investigated. The synthesized particles, being formed after heat-treatment at 900°C for 16 h, showed a well-crystallized morphology. Under the excitation at 980 nm, CaGd2(- MoO4)4:Er3+/Yb3+ particles exhibited strong 525 and 550-nm emission bands in the green region and a weak 655-nm emission band in the red region. The Raman spectrum of undoped CaGd2(MoO4)4 revealed about 15 narrow lines. The strongest band observed at 903 cm– 1 was assigned to the m1 symmetric stretching vibration of MoO4 tetrahedrons. The spectra of the samples doped with Er and Yb obtained under 514.5 nm excitation were dominated by Er3+ luminescence preventing the recording Raman spectra of these samples. Concentration quenching of the erbium luminescence at 2H11/2?4I15/2 and 4S3/2?4I15/2 transitions in the CaGd2(MoO4)4:Er3+/Yb3+ crystal structure was established to be approximately at the 10 at.% doping level. | |
Ссылка на другой сайт | http://onlinelibrary.wiley.com/doi/10.1111/jace.13739/abstract | |
Тема | Sol–Gel Synthesis | |
Тема | Upconversion. Photoluminescence | |
Тема | Raman | |
Название | Microwave Sol–Gel Synthesis of CaGd2(MoO4)4:Er3+/Yb3+ Phosphors and Their Upconversion Photoluminescence Properties | |
Тип | Journal Article | |
Тип | Journal Article Preprint | |
Страницы | 3223-3230 | |
ГРНТИ | 29.31.26 | |
Дата обновления | 2016-11-11T08:54:04Z | |
DOI | 10.1111/jace.13739 | |
Подразделение | Научно-исследовательская часть | |
Журнал | Journal of the American Ceramic Society | |
Квартиль журнала в Scopus | Q1 | |
Квартиль журнала в Web of Science | Q1 |