Investigation of Electrical Characteristics of High Temperature Ceramic-Metal Contact Assemblages
Скачать файл:
URI (для ссылок/цитирований):
https://elib.sfu-kras.ru/handle/2311/1446Автор:
Kirko, Vladimir I.
Stepanov, Egor I.
Nagibin, Gennady E.
Dobrosmislov, Sergey S.
Gusev, Alexander O.
Simakov, Dmitry A.
Дата:
2009-09Аннотация:
There was carried out research work on electrical technical characteristics of contact assemblages
made of materials with very diverse linear expansion coefficients (LECs) at temperatures up to 900°С
and current loads of long-durations up to 100 hours. Foam nickel was employed as a conductive
damping material. After being subjected to long current and heat loads contact junctions between the
foam nickel and contact assemblage materials were studied by scanning electron microscopy (SEM)
and X-ray diffraction (XRD) analysis.